Aluminium Filler Wire

Aluminium Filler Wire Manufacturers, Suppliers And Exporter

Aluminium Filler Wire : Although many metals are TIG welded, the metal most frequently associated with the process is aluminum, especially with metals of a smaller thickness. Many other processes, of course, can join aluminum, but in the lighter gauges the most applicable process is TIG. The popularity of aluminum in automotive applications has brought TIG welding to a new golden age. Mechanically strong and visually appealing, TIG welding is the number one process chosen by professional welders for professional racing teams, and the avid auto enthusiast or hobbyist.

With the active support of our team of experts, we are engaged in offering a huge gamut of Aluminum Filler Wire. This Aluminum Filler Wire is specially designed and developed to meet all the needs of our international clients. We take into account the international quality standards set by the industry and offer suitable range of Aluminum Filler Wire. This Aluminum Filler Wire is widely appreciated among our huge client base at Ahmedabad, Bangalore, Chennai, Mumbai, Surat, Vadodara, Gujarat And all over India.

Grade Size
(mm)
Typical Analiysis of Filler Wire Typical All Weld Mechanical Properties Applications
AI Si Mn Fe Mg Cu Y.P.
N/mm2
(Ksi)
T.S.
N/mm2
(Ksi)
EI.
(%)
as welded brinnel hardness
ER4043 TIG
1.6
2.0
2.4
4.0
Length
1000
MIG
0.6
0.8
0.9
1.0
1.2
1.6
Bal. 4.5-6.0 0.05
max
0.80
max
0.05 0.30
max
200
(29)
For welding 3003,3004,5052,6061, 6063 and casting alloys 43, 355, 356 and 214.
ER4047 Bal. 11.0-
13.0
0.15 max 0.80 max 0.10 0.30 max 190
(27.5)
For welding 1060, 1350, 3003, 3004, 3005, 5005, 5050, 6053, 6061, 6951, 7005and cast alloys 710.0 and 711.0. Provides good corrossion resestance.
ER5356 Bal. 0.25 0.05-0.20 0.40 max 4.5-5.5 0.10 max 26
(3.8)
For welding 5050, 5052, 5083, 5356, 5454, 5456. Provides much better corrossion resistance to salt water.
ER1100 99 min. Fe&Si 0.95 max 0.50 max Fe&Si0.95 0.05-0.20 93
(13.5)
For architectural or decorative application. For welding 1100, 3003, 3003 to 1060, to 1080, to 1350.
ER5183 Bal 0040 0.50-1.0 0.40 4.3-5.2 0.10 It is most frequently used on 5083 base plate. It is also used to weld 6061, 6063, 5086, 7005 and 7039 alloys